Use of Aluminium
Chris,
Don't see any reason why you couldn't use Aluminium for the test provided the diameter of the bar was increased. The overhang for the test (assuming it's no more than say 100mm or 4") isn't enough to cause any concerns about deflection provided you take very light cuts. Heavy cuts will push the bar away from centre and give you readings where you'll begin chasing your tail.
The ToT recommends using 1" (25mm) "soft steel" - which means annealed or normalised plain carbon. Assuming you're planning on using 20mm steel bar for the test, you'd need to go to about 30mm for Aluminium in order to give you the same stiffness, which means the same amount of deflection due to machining in each case. Hope this makes sense - if not PM me.
David
-
21st November 2011 05:43 PM # ADSGoogle Adsense Advertisement
- Join Date
- Always
- Location
- Advertising world
- Posts
- Many
-
21st November 2011, 09:26 PM #32GOLD MEMBER
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 2,637
Thanks for the feedback David.
Similar Threads
-
Taper turning attachment for Hercus
By ljvs1951 in forum THE HERCUS AREAReplies: 18Last Post: 5th December 2010, 08:26 PM -
Hercus Text Book of Turning
By new_guy90 in forum THE HERCUS AREAReplies: 4Last Post: 14th April 2010, 12:10 AM -
Hercus 9" vs hercus 260 ????????
By bitza500 in forum THE HERCUS AREAReplies: 1Last Post: 26th June 2009, 10:50 PM -
Wood Turning Toolpost for Hercus
By Big Shed in forum THE HERCUS AREAReplies: 2Last Post: 15th April 2009, 10:24 PM