"finishing both sides of a board in the same...
"finishing both sides of a board in the same manner prevents differential moisture loss, so minimises warping and cupping ... so the next best thing is probably a polyurethane varnish" This makes...
-
19th September 2018, 10:10 AM
- Replies
- 6
- Views
- 1,434
Thanks for the tip Arron. The underside of the...
Thanks for the tip Arron. The underside of the desk feels raw to the touch so does inside the desk. Should I oil that? Or since its not a work surface would one normally not bother - I'm mostly...
-
17th September 2018, 03:33 PM
- Replies
- 6
- Views
- 1,434
mineral oil over nitrocellulous on mango desk
Hi All
I purchased a lovely kiln-dried mango-wood desk. I read that without maintenance, mango is prone to drying and cracking in dry climates with heating, particularly near radiators. I live in...