    Default casting resin questions

    Hi all

    Just getting to the final stages of a hall table from beautiful recycled Aussie mahogany (euc resinafera?) and I had a couple of questions about using resins to fill holes.

    Dumb question 1. do you use the resin before sanding and other finishing?

    Dumb question 2. If yes above, does sanding 'cloud' the surface of the resin? I want it quite clear?

    Dumb question3. How on earth do you measure 2.5 ml that you need of the catalyst? Is it a few drops? Or should I try to get a syringe from a junkie? Or maybe a chemist? I understand that you need to be pretty accurate, but I'm not sure exactly how.

    Thanks

    Trav
    Some days we are the flies; some days we are the windscreen

  2. # ADS
    Google Adsense Advertisement
    Join Date
    Always
    Location
    Advertising world
    Age
    2010
    Posts
    Many





     
  3. #2
    Join Date
    Apr 2004
    Location
    Canberra
    Posts
    431

    Default

    Sorry don't know about DQ1&2, but syringes are freely available at chemists now. The only thing to check is the solvent compatability, but they are pretty resistant to most things, they do not handle chloroform or acetonitrile real well.

  4. #3
    Join Date
    Jul 2003
    Location
    British Columbia, Canada
    Posts
    110

    Default

    Sand the resin along with the rest of the project. The resin will appear clear when the final finish is applied, eg. varnish, etc.

    If the resin is applied after the sanding it will never be as flat as the rest of the surface.
    Keep flying until every bit falls off.

  5. #4
    Join Date
    Apr 2002
    Location
    Brisbane
    Posts
    5,773

    Default

    syringes are quite fine for epoxy hardners.
    The only problem is cleaning them, so don't.
    The chemist will look less funny at you if you explain what you need them for & specify that you don't require any sharps.
    5mL syringes are a realy handy to have arround the workshop.
    Want to ge some PVA into that cracked timber, easy with a syringe.
    Any thing with sharp teeth eats meat.
    Most powertools have sharp teeth.
    People are made of meat.
    Abrasives can be just as dangerous as a blade.....and 10 times more painfull.

  6. #5
    Join Date
    Jan 2004
    Location
    Over there a bit
    Age
    17
    Posts
    2,511

    Default

    Is this abad time to mention I buy both 2ml and 5ml syringes as well as 20ml syringes by the box?
    Boring signature time again!

  7. #6
    Join Date
    May 1999
    Location
    Tooradin,Victoria,Australia
    Age
    73
    Posts
    11,918

    Default

    Quote Originally Posted by outback
    Is this abad time to mention I buy both 2ml and 5ml syringes as well as 20ml syringes by the box?
    I have often wondered what drives you.

  8. #7
    Join Date
    Apr 2005
    Location
    Nerang Queensland
    Age
    66
    Posts
    10,766

    Default

    Quote Originally Posted by Trav
    Dumb question 1. do you use the resin before sanding and other finishing?

    Dumb question 2. does sanding 'cloud' the surface?

    Dumb question3. How on earth do you measure.
    1. Use the resin before finishing, and before or during sanding (I use before final sanding). If you overcast, using well of puty etc, I've found it better to grind back majority of resin with dremmel or file. You can turn the resin also, but often at can fracture and you may need to recast small areas.
    2. No. As Canfly says, it will become clear on finishing.
    3. I tend to always mix too much and then get quantities right. Too little catalyst and you will have a sticky mess, too much also causes problems. Better to waist some than waist your time doing it all again.

    With smaller cracks you could also use the thick CA glue with accelerator to save the resin, but on the other hand, CA costs more. With very big cracks/holes, remember to cast the resin in small layers, large pours will crack and pull away from the sides due to shrinkage.

    Hope this helps.

    Cheers
    Neil
    ____________________________________________
    Every day presents an opportunity to learn something new

  9. #8
    Join Date
    Nov 2004
    Location
    Port Pirie SA
    Age
    52
    Posts
    6,908

    Default

    Neil, what would you call a large pour.
    I have some knots/nail holes to fill up some about the size of a 20c piece upto 10mm deep.
    ....................................................................

  10. #9
    Join Date
    Jan 2004
    Location
    Over there a bit
    Age
    17
    Posts
    2,511

    Default

    Quote Originally Posted by
    I have often wondered what drives you.
    Yeh man, I just wake up in the morning and decide how big a kick start I need to face the world.
    Boring signature time again!

  11. #10
    Join Date
    Oct 2003
    Location
    Canberra
    Age
    48
    Posts
    1,484

    Default

    Thanks everyone.

    Just to follow up on Harry72's comment, how big a hole is it before it becomes too much to pour in one go? I'm trying to make a feature out of a big knot in the wood - it is mostly filled by timber, but there is a fair bit of cavity there. Not quite as big as Harry72's hole, but close.

    Trav
    Some days we are the flies; some days we are the windscreen

  12. #11
    Join Date
    May 2005
    Location
    Magill, Adelaide
    Age
    59
    Posts
    1,537

    Default

    Interesting stuff to read about fellas. Never knew about resin until today.

    Syringes can be picked up at your pharmacist but they wont give you needles, which is OK because glue and stuff just won't go through a needle *G*

    Just a thought that measuring cups for various medicines would work too.

    A syringe is a great tool to have as it allows you to precisely place the glue resin whatever on the job

    Stevo

  13. #12
    Join Date
    Apr 2005
    Location
    Nerang Queensland
    Age
    66
    Posts
    10,766

    Default

    Quote Originally Posted by Harry72
    what would you call a large pour ... I have some knots/nail holes to fill up some about the size of a 20c piece upto 10mm deep.
    That size should be no problem. I've read somewhere else you can pour up to 10mm thick and I've had no problems up to that size. I use Diggers clear casting resin from Bunnies. When you get too big you'll know it, especially if you have to much catalyst, but you can always pour some more to fill the cracks and/or shrinkage.
    Neil
    ____________________________________________
    Every day presents an opportunity to learn something new

  14. #13
    Join Date
    Mar 2004
    Location
    Hornsby, NSW
    Age
    49
    Posts
    453

    Default

    My local Bunnies stocks the Diggers Resin but not the catalyst and I got a blank look when I asked where the catalyst was.
    If I do not clearly express what I mean, it is either for the reason that having no conversational powers, I cannot express what I mean, or that having no meaning, I do not mean what I fail to express. Which, to the best of my belief, is not the case.
    Mr. Grewgious, The Mystery of Edwin Drood - Charles Dickens

  15. #14
    Join Date
    May 2005
    Location
    Hamilton, New Zealand
    Age
    58
    Posts
    61

    Default

    A good place to get resin is a fibreglass shop. They normally have a wide range and will have an very good knowledge of pros and cons. Knowledge of these types of products is not normally found at my local Bunnings (though the product is!!).

    Recently used resin to fill some knots and holes in a table I have been making. Once finish applied has come up outstanding. Used Epiglass HT9000, easy to use.

    Good luck
    Regards

    Pete

  16. #15
    Join Date
    Feb 2004
    Location
    Adelaide Hills
    Posts
    821

    Default

    I used pouring resin from a craft shop,

    the knot holes I'm filling in are not not all that large but are deep. I poured the resin in stages so as to allow it time to cure.

    One thing to look out for is to make sure you plug the other end of the hole if it goes tight through the timber. DAMHIK :eek:

    I haven't gotten around to sanding yet but decided to take the suck it and see aproach. I figure if it doesn't come out right then I can sart again.

    Himzo
    There's no such thing as too many Routers

Page 1 of 2 12 LastLast

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •