    Hi everyone

    David has just finished a scroll sawn chess set. The 'white' men are made from Pawlonia, which is not really white, but is sufficiently so to contrast with the red gum 'black' men. This timber is very soft and fragile, so finishing needs to be done gently. David has done a sample piece with oil and naturally this has turned the piece quite yellow.

    So here's the thing - is there any sort of finish that can be applied to keep that whiteness in tact? The Pawlonia is not particularly interesting visually, so the finish really is only needed to give it some protection from soiling. If the pieces need to be painted, that would fall to me, whether its a sealer type of finish, or a decorative one, and quite frankly I don't fancy the job. So, the easier the process, the better.


  2. # ADS
    Google Adsense Advertisement
    Join Date
    Always
    Location
    Advertising world
    Posts
    Many





     
  3. #2
    Join Date
    Oct 2006
    Location
    Melbourne
    Posts
    5,271

    Default

    Bleached shellac is about as transparent and colourless as it gets for a simple DIY finish. You could also add some pigment to the shellac to increase the whiteness. Titanium white is about as bright white as it gets.
    .
    I know you believe you understand what you think I wrote, but I'm not sure you realize that what you just read is not what I meant.


    Regards, Woodwould.

  4. #3
    Join Date
    Aug 2008
    Location
    Deniliquin - Southern Riverina
    Posts
    313

    Default

    Thanks Woodwould
    When using shellac, can I use water based pigments to colour, or do I need to use powder? I have artist's quality watercolour paint in Titanium white.

  5. #4
    Join Date
    Oct 2006
    Location
    Melbourne
    Posts
    5,271

    Default

    Your water based white would be fine under shellac once it's fully dry.
    .
    I know you believe you understand what you think I wrote, but I'm not sure you realize that what you just read is not what I meant.


    Regards, Woodwould.

  6. #5
    Join Date
    Aug 2008
    Location
    Deniliquin - Southern Riverina
    Posts
    313

    Default

    Thanks so much. Problem solved and so quickly.

  7. #6
    Join Date
    Jun 1999
    Location
    Westleigh, Sydney
    Age
    77
    Posts
    9,550

    Default

    To add to what WW said, shellac is probably the easiest finish to apply, and (if necessary) repair. That probably won't be a problem for chess pieces.
    Visit my website
    Website
    Facebook

  8. #7
    Join Date
    Aug 2008
    Location
    Deniliquin - Southern Riverina
    Posts
    313

    Default

    Thanks Alex. Makes me even happier. I'm finding finishing quite tedious at the moment, so if my experience with shellac is good, it might become the finish of my choice in future. Just have to get hold of some. None here in the bush, so it's back to the net again.

  9. #8
    Join Date
    Oct 2006
    Location
    Melbourne
    Posts
    5,271

    Default

    Try our illustrious leader's stuff. Jim Carroll sells it on his site too.
    .
    I know you believe you understand what you think I wrote, but I'm not sure you realize that what you just read is not what I meant.


    Regards, Woodwould.

  10. #9
    Join Date
    Dec 2008
    Location
    Eastern Australia
    Posts
    604

    Default

    To add to this. What you must do is understand why wood changes colour. Red gum off the saw has lovely shades of pink. Given time these turn to the red we expect from the species.
    This is oxidisation, basicially the wood is rusting. Now for wood to yellow, sorry Im not sure of the chemestry. What I do know is that paint will yellow if it does not have enough UV light.
    So is there a fix, and is the fix some varnish, I doubt that, But *I would never discourage shellac as a product, its easy and quick, and a failure is fairly easy to remedy.

Similar Threads

  1. Yellowing Effect
    By bdar in forum WOODTURNING - PEN TURNING
    Replies: 9
    Last Post: 13th June 2007, 12:02 AM
  2. Danish Oil Yellowing
    By Bruce Wilson in forum FINISHING
    Replies: 3
    Last Post: 13th March 2007, 08:29 PM
  3. Preventing Pine From Yellowing
    By Sir Stinkalot in forum FINISHING
    Replies: 3
    Last Post: 11th May 2006, 10:25 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •